Titanium alloy can not only make marine equipment develop towards "deep, large, far, high ", but also fully realize the same life as the main body of marine equipment. It is the best choice for marine equipment. At present, China pays more attention to the application of titanium in marine equipment, and the amount of titanium used is also increasing. Deep-sea pressure shell, seawater pipeline, cylinder superstructure, frame, etc. will become the key development direction of marine titanium.

V súčasnosti existuje veľa aplikácií titánu v lodnom priemysle doma iv zahraničí.
However, the material system in relevant specifications is not perfect. It is hoped that relevant units will organize discussion and improve the material system in current relevant codes such as Titanium Pressure Vessel, Material and Welding, so as to facilitate the designer's reference.
Upper buildings:
V súčasnosti existuje niekoľko príkladov použitia v nadstavbe domácich vojnových lodí, ako napríklad Ti70 (TA23) pre stožiar, tyč TA5 a TA7 pre anténu radaru, platňa TA2 a TA5 pre plášť hangáru a rámová konštrukcia.
Titán sa vo veľkej miere používa aj v horných stavebných priestoroch obojživelnej prístavnej lode LPD17, čím sa znížila jej hmotnosť asi o 50 percent a výrazne sa zlepšila jej stabilita.
Výrobné aplikácie v iných oblastiach
Okrem veľkého množstva titánu použitého vo vyššie uvedenom -tlaku odolnom kryte, potrubnom systéme a nadstavbe sú v námorných zariadeniach doma aj v zahraničí užitočné aj ďalšie komponenty.